Nanocyl PLASTICYL™ PC1501 Polycarbonate - Carbon Nanotube Masterbatch

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Conductive
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ PC1501 Polycarbonate - Carbon Nanotube Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PC1501 is a conductive masterbatch based on polycarbonate. Because of its low viscosity and high flow formulation, PLASTICYL™ PC1501 is ideal for standard injection molding and extrusion processes.Key Applications:E&E, automotive and packaging industriesHDD (hard disk drive) internal componentsHDD and IC handling traysBenefits:Excellent electrical conductivity at low loadingExcellent surface cleanlinessRetention of key mechanical propertiesEase of processing
Physical Properties Metric English Comments
Specific Gravity 1.175 g/cc
1.175 g/cc
ISO 1183
Filler Content 14 - 16 %
14 - 16 %
Carbon Nanotube Loading
High Load Melt Index <= 5.6 g/10 min

@Load 20.0 kg,
Temperature 300 °C
<= 5.6 g/10 min

@Load 44.1 lb,
Temperature 572 °F
4 mm; Non-standard Test
Processing Properties Metric English Comments
Processing Temperature 300 °C
572 °F
Material Temperature
Hold Pressure 45.0 MPa
6530 psi
Back Pressure 4.00 MPa
580 psi
Descriptive Properties Value Comments
Processing: Holding Time 8 s
Processing: Injection Speed 30 cm³/s
Processing: Plasticizing Speed 0.4 m/s