Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate with 5 wt% Multi-Wall Carbon Nanotubes

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Carbon Fiber Filled
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate with 5 wt% Multi-Wall Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PBT1501 is a conductive masterbatch based on polybutylene terephthalate. Because of its high flow formulation, PLASTICYL™ PBT1501 is ideal for standard injection molding and extrusion processes.Applications:ESD (Electrostatic Discharge) and electrically conductive partsE&E, automotive, industrialInjection molding, extrusionBenefits:Electrical conductivity at low loadingRetention of key mechanical propertiesEasier processing
Physical Properties Metric English Comments
Filler Content 5 %
5 %
Carbon Nanotube Loading
Melt Flow 5.51 g/10 min

@Load 5.00 kg,
Temperature 250 °C
5.51 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ISO 1133:1997
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
Masterbatch; ISO 11357-1,-3
Electrical Properties Metric English Comments
Volume Resistivity 30 ohm-cm
30 ohm-cm
Approximate value obtained from graphical representation; CTM E043
Surface Resistivity per Square 70 ohm
70 ohm
Approximate value obtained from graphical representation; CTM E042