Nanocyl PLASTICYL™ HDPE1501 High Density Polyethylene - Carbon Nanotube Masterbatch

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ HDPE1501 High Density Polyethylene - Carbon Nanotube Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ HDPE1501 is a conductive masterbatch based on high density polyethylene. Because of its flow formulation, PLASTICYL™ HDPE1501 is ideal for standard injection molding and extrusion processes.Applications:ESD (Electrostatic Discharge) and electrically conductive partsE&E, automotive, industrialInjection molding, extrusionBenefits:Electrical conductivity at low loadingRetention of key mechanical propertiesEasier processing
Physical Properties Metric English Comments
Specific Gravity 0.977 g/cc
0.977 g/cc
ISO 1183
Filler Content 14 - 16 %
14 - 16 %
Carbon Nanotube Loading
High Load Melt Index <= 7.84 g/10 min

@Load 20.0 kg,
Temperature 260 °C
<= 7.84 g/10 min

@Load 44.1 lb,
Temperature 500 °F
4 mm; Non-standard Test
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
ISO 11357-1,-3