Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6

Category Polymer , Thermoset , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Nanocyl
Trade Name EPOCYL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EPOCYL™ NC R128-04 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of 6. It is specifically developed to enhance the mechanical properties of the final fiber reinforced composite materials. Special features include easy integration and great flexibility in design of new multifunctional materials.Applications: High performance structural composite partsAutomotive (bumpers and other structural parts)Marine, especially sailing boats (structural outer shell in carbon fiber composite, masts and other generic structural parts)Industrial parts (rollers, doctor-blades and wind-mill blades)Sporting equipments (bike frames, hockey sticks, tennis rackets, skis and golf shafts)Aerospace (structural parts and interiors)Main direct advantages (demonstrated in specific final formulation)Improved fracture toughness (G1C) of over 100% = higher crack propagation/delamination resistanceImproved failure strength: transverse and off-axis (+/- 45°) by over 15% = higher shear resistanceReduced CTE of over 15% = less distorted parts producedNo reduction in the Tg = possible to be used in any formulationAdditional advantages in generalElectrical properties: induces antistatic properties in the composite parts; excellent for electrostatic painting applicationFlame resistance: higher resistance to flammability up to UL 94 level on the final fiber reinforced compositeBetter thermal dissipation: avoids hot-spots during curing, more homogenous temperatureCuring agents EPOCYL™ NC R128-04 can be cured or cross-linked with different types of curing agents depending on the properties desired in the final composite like any conventional Bis-A based formulations.IMPORTANT: EPOCYL™ NC R128-02 is not an additive in your formulation, it is a substitution product for the equivalent parts of your conventional Bis A liquid resin. EPOCYL™ NC R128-02 is designed only for formulating solvent based formulations.
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.20 g/cc
1.15 - 1.20 g/cc
Viscosity 25000 - 45000 cP

@Temperature 25.0 °C
25000 - 45000 cP

@Temperature 77.0 °F
Descriptive Properties Value Comments
Aspect Paste, black (Master Batch)
Epoxy Equivalent 196.1 - 203.52 g/eq
Epoxy Value 4.91 - 5.1 eq/kg
Storage Temperature 5°C - 40°C
Users viewing this material also viewed the following: