NanoScale NanoActive® Aluminum Oxide

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer NanoScale
Trade Name NanoActive®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoScale NanoActive® Aluminum Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NanoActive Al2O3 is produced using proprietary processes to obtain high specific surface area, low density, amorphous material with high adsorption capacity and chemical reactivity. NanoActive Al2O3 can be dispersed in various carrier fluids with greatly reduced particle sizes.Applications: Applications include air cleaning, capacitors, catalysts supports, coatings, heat transfer fluids (suspensions), polishing materials, polymer nanocomposites for improved tribological performance, and structural ceramics.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
Density 3.90 g/cc
0.141 lb/in³
Loss On Ignition 2.1 %
2.1 %
Particle Size 1.5 µm
1.5 µm
mean aggregate size
Specific Surface Area >= 275 m²/g
>= 275 m²/g
BET
Pore Size 0.00280 microns
0.000110 mil
Average Diameter
Component Elements Properties Metric English Comments
Aluminum, Al >= 99.8 %
>= 99.8 %
Descriptive Properties Value Comments
Appearance / Color White Powder
Crystallite Size Amorphous
Minimum Total Pore Volume cc/g 0.15