Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a greater service life than standard grades of glass reinforced Nylon 6. NYCOA ASN 27 300 KNF is available in UV stable, custom colors, and impact modified grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons. Typical applications include automotive pedals, power tool housing, and lawn & garden equipment parts.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 178 MPa
25800 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 9.45 GPa
1370 ksi
ASTM D638
Flexural Strength 210 MPa
30500 psi
ASTM D790
Flexural Modulus 8.22 GPa
1190 ksi
ASTM D790
Izod Impact, Notched 1.35 J/cm
2.53 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648