plasticized and heat stabilized extrusion grade for the wire jacketing industry to 3,000 fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.0 MPa
11500 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.585 GPa
374.9 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 220 °C
428 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Drying Temperature 76.0 °C
169 °F