Material Notes:
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the production of insulation plaster.Applications: This grade is used to produce insulation plaster by mixing pre-expanded beads with plaster.This grade should not be used for food contact applications.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density >= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Bead Size 0.200 - 0.400 mm
0.00787 - 0.0157 in
0.200 - 0.400 mm
0.00787 - 0.0157 in
Breda Laboratory Analytical Methods 90.30
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Breda Laboratory Analytical Methods 90.16
Blowing Agent Content >= 5.9 %
>= 5.9 %
Breda Laboratory Analytical Methods 90.18