NOVA Chemicals Sclair® IG454-A Injection Molded HDPE Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® IG454-A Injection Molded HDPE Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IG454-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG454-A is subject to the specific limitation that it may contact food only at temperatures of 212°F and below.NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Superior stiffness allows for part thinwalling and enhanced stacking strength, Lower viscosity for exceptional processability yielding shorter cycle times and energy savings, Exceptional solid state properties provide improved impact resistance and ESCR, Good organoleptic properties and natural colorAdditives: AntioxidantApplications: Shipping pails (both food and industrial), Storage bins and totes, Caps and closures, Crates
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
50 mm/min test speed; ASTM D 638
Tensile Strength, Yield 22.3 MPa
3230 psi
50 mm/min test speed; ASTM D 638
Elongation at Break 650 %
650 %
50 mm/min test speed; ASTM D 638
Elongation at Yield 9.0 %
9.0 %
50 mm/min test speed; ASTM D 638
Flexural Modulus, 1% Secant 960 MPa
139000 psi
ASTM D 790