Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good ESCR, high stiffness, good impact strength.Applications: Small part blow molding, HIC containers, food, pharmaceuticals.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance 100 hour
100 hour
F50, Condition A, ASTM D1693
Melt Flow 0.41 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.41 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 50 %
50 %
at 500 mm/min; ASTM D638
860 %
860 %
at 50 mm/min; ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 160 - 205 °C
320 - 401 °F