Material Notes:
Features: Medium molecular weight, excellent ESCR, excellent toughness, good processability, good chemical resistance.Applications: Extrusion on to metal pipes to produce a corrosion resistant coating for buried pipe systems.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ASTM D792
Environmental Stress Crack Resistance 1000 hour
1000 hour
Melt Flow 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Modulus 0.580 GPa
84.1 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
ASTM D3417
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D696
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.34
2.34
ASTM 1531
Dissipation Factor 0.00050
0.00050
ASTM 1531
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F