NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 0.72 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.72 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 800 %
800 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Secant Modulus, MD 0.210 GPa
30.5 ksi
ASTM D882
Secant Modulus, TD 0.230 GPa
33.4 ksi
ASTM D882
Coefficient of Friction 0.20
0.20
ASTM D1894
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 20.0 g/micron
508 g/mil
ASTM D1922
Dart Drop 3.00 g/micron
76.2 g/mil
F 50; ASTM D1709/A
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
ASTM D882
Film Tensile Strength at Break, TD 31.0 MPa
4500 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D696
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 0.0250 mm
6.0 %

@Thickness 0.000984 in
ASTM D1003
Gloss 65 %
65 %
45°; 1 mil; ASTM D1894
Processing Properties Metric English Comments
Melt Temperature 220 - 230 °C
428 - 446 °F