Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® LM-0724-A LDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® LM-0724-A LDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LM-0724-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biologically and chemically inert.Features: Excellent balance of stiffness and toughness, Good processability and dimensional stabilityApplications: Caps and closures, including tamper evident closures
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D 792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D 2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D 638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D 638
Elongation at Break 500 %
500 %
ASTM D 638
1% Secant Modulus 345 MPa
50000 psi
ASTM D 790
2% Secant Modulus 0.305 GPa
44.2 ksi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 97.0 °C
207 °F
ASTM D 1525
Users viewing this material also viewed the following: