Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D792
Water Absorption 0.010 %
0.010 %
ASTM D570
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50; ASTM D1693
Oxidative Induction Time (OIT) 10 min
10 min
ASTM D3895
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
ASTM D3417
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Copyright © lookpolymers.com All Rights Reserved