NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 170 hour
>= 170 hour
F50, Condition B, ASTM D1693, 100% Igepal
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -85.0 °C
<= -121 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 160 - 205 °C
320 - 401 °F
Copyright © lookpolymers.com All Rights Reserved