NOVA Chemicals Novapol® HB-W646-U HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-W646-U HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High molecular weight HDPEExcellent ESCRImpact strengthGood processability Applications: DrumsJerry cansIBCsMarine fuel tanksInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D792
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A; ASTM D1693
>= 1000 hour
>= 1000 hour
Condition B; ASTM D1693
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 840 %
840 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 4.00 J/cm

@Thickness 3.20 mm
7.49 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
F<sub>50</sub>, notched specimen; ASTM D746