Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High molecular weight, High rigidity, Excellent impact strength, Excellent ESCR, Used in high purity chemical packagingInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50 mm/min; ASTM D638
Elongation at Break 830 %
830 %
50 mm/min; ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
at 1% Secant; ASTM D790
Izod Impact, Notched 7.20 J/cm

@Thickness 3.20 mm
13.5 ft-lb/in

@Thickness 0.126 in
ASTM D256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F