Fast acting anaerobic primer. On part life 7 days. Non-ozone depleting but flammable solvent
Physical Properties Metric English Comments
Viscosity 3.0 cP
3.0 cP
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
On metal (Fixture)
360 min
6.00 hour
On metal (Full)
Descriptive Properties Value Comments
Color Yellow
Users viewing this material also viewed the following: