ND Industries 440 High pressure Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries 440 High pressure Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pneumatic and hydraulic sealant fluid, for power and gas system connections
Physical Properties Metric English Comments
Viscosity 12000 - 16000 cP
12000 - 16000 cP
Mechanical Properties Metric English Comments
Shear Strength >= 68.9 MPa
>= 10000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min
0.500 hour
With Primer (Fixture)
240 min
4.00 hour
On steel (fixture)
1440 min
24.0 hour
On Steel (Full)
1440 min
24.0 hour
With Primer (Full)
Descriptive Properties Value Comments
Color Purple