Material Notes:
Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Electrical Appliances Toys Industry AutomobileInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
NCMT Method
Melt Flow 32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.0 MPa
3630 psi
ASTM D638
Elongation at Break >= 80 %
>= 80 %
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Deflection Temp.; ASTM D648