NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
NCMT Method
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Elongation at Break <= 60 %
<= 60 %
ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
ASTM D638
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Deflection Temp.; ASTM D648