Material Notes:
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
NCMT Method
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ASTM D638
Elongation at Break <= 600 %
<= 600 %
ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM D638
Izod Impact, Notched 1.68 J/cm
3.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Deflection Temp.; ASTM D648