Material Notes:
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
NCMT Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Tensile Modulus 3.20 GPa
464 ksi
ASTM D638
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection Temp.; ASTM D648