NAPCO C95 Magnesite

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer NAPCO
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NAPCO C95 Magnesite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dead burned refractory grade magnesite from the Liaoning province of China. Data provided by the manufacturer, North American Processing Company.
Physical Properties Metric English Comments
Loss On Ignition <= 0.60 %
<= 0.60 %
Component Elements Properties Metric English Comments
Al2O3 0.50 %
0.50 %
CaO 1.4 %
1.4 %
Fe2O3 0.60 %
0.60 %
MgO 95.2 %
95.2 %
SiO2 1.6 %
1.6 %