Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polypropylene (PP)
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications and is particularly well suited for thin wall bumper fascias applications.Key Applications: Bumper fascias, cladding and bodyside moldingInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 26 g/10 min
26 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
15 sec; ISO 868
Tensile Strength, Yield 17.0 MPa
2470 psi
50 mm/min; ISO 527
Flexural Modulus 1.73 GPa
251 ksi
Chord; 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ISO 75-1