Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648