Mytex Polymers AS65KW-LG Polypropylene, Talc filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS65KW-LG Polypropylene, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: Non-painted instrument panelInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Ash 25 %
25 %
ASTM D5630