Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good impact performance properties.Key Applications: Automotive exteriorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Melt Flow 17 g/10 min
17 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
15 sec; ISO 868
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min; ISO 527
Flexural Modulus 1.35 GPa
196 ksi
Tangent; 1.3 mm/min; ISO 178
Izod Impact, Notched (ISO) 40.0 kJ/m²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1