Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Yield 27.0 MPa
3920 psi
50 mm/min; ASTM D638
Flexural Modulus 1.75 GPa
254 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 0.660 J/cm

@Temperature 23.0 °C
1.24 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved