Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Material ”S”® 8000 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Material ”S”®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Material ”S”® 8000 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding guides, slide segments, and slide bearings.Special Properties:• Self-lubricating - lower sliding friction coefficient• Increased wear resistance• Excellent impact/shock resistance• Good resistance to chemicals• Good anti-adhesion properties• Electrically isolating• Better resistance to UV rays than Original Material ”S”® green/naturalInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 0.930 g/cc
<= 0.0336 lb/in³
ISO 1183
Molecular Weight 9.00e+6 g/mol
9.00e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
DIN 53505
Ball Indentation Hardness 43.0 MPa
6240 psi
Tensile Strength 21.1 MPa
3060 psi
ISO 527
Elongation at Break 265 %
265 %
ISO 527
Modulus of Elasticity 0.700 GPa
102 ksi
Charpy Impact, Notched >= 17.0 J/cm²
>= 80.9 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
0.10 - 0.20
Sand Slurry 90
90
value in %
Thermal Properties Metric English Comments
CTE, linear 170 µm/m-°C

@Temperature 23.0 - 60.0 °C
94.4 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -200 °C
-328 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Strength <= 45.0 kV/mm
<= 1140 kV/in
IEC 60243
Descriptive Properties Value Comments
Color Anthracite
Copyright © lookpolymers.com All Rights Reserved