Murlin Natural Bone Ash Mold Release

Category Ceramic , Wood and Natural Products
Manufacturer Murlin Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murlin Natural Bone Ash Mold Release.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Bone ash is used as a mold release agent.Information provided by Murlin Chemical, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0369 lb/in³
Loss On Ignition <= 1.5 %
<= 1.5 %
Ash 0.60 %
0.60 %
Acid Insoluble Ash
99.5 %
99.5 %
Soluble Ash
Component Elements Properties Metric English Comments
CaO 54.8 %
54.8 %
CO2 1.1 %
1.1 %
MgO 1.1 %
1.1 %
P2O5 40.9 %
40.9 %
SiO2 <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Color White
P2O5 40.9%
Screen 95% minus 325