Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
as molded
63
63
post cured- 2 hours at 177°C
72
72
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 6.03 MPa
875 psi
post cured- 4 hours at 204°C
7.58 MPa
1100 psi
post cured- 2 hours at 177°C
7.86 MPa
1140 psi
as molded
Tensile Strength, Yield 2.76 MPa
400 psi
at 200%, as molded
3.07 MPa
445 psi
at 200%, post cured- 2 hours at 177°C
3.31 MPa
480 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 511 %
511 %
post cured- 4 hours at 204°C
590 %
590 %
post cured- 2 hours at 177°C
663 %
663 %
as molded
Tear Strength 37.2 kN/m
212 pli
post cured- 4 hours at 204°C; Die B
42.2 kN/m
241 pli
post cured- 2 hours at 177°C; Die B
47.0 kN/m
268 pli
as molded; Die B