Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
as molded
51
51
post cured- 2 hours at 177°C
55
55
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 9.825 MPa
1425 psi
post cured- 4 hours at 204°C
10.63 MPa
1542 psi
as molded
11.05 MPa
1602 psi
post cured- 2 hours at 177°C
Tensile Strength, Yield 2.69 MPa
390 psi
at 200%, as molded
3.03 MPa
440 psi
at 200%, post cured- 2 hours at 177°C
3.24 MPa
470 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 538 %
538 %
post cured- 4 hours at 204°C
596 %
596 %
post cured- 2 hours at 177°C
650 %
650 %
as molded
Tear Strength 26.5 kN/m
151 pli
post cured- 4 hours at 204°C; Die B
33.8 kN/m
193 pli
post cured- 2 hours at 177°C; Die B
38.9 kN/m
222 pli
as molded; Die B