Multibase SILASTIC® C7-4550 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4550 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 51
51
as molded
51
51
post cured- 2 hours at 177°C
51
51
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 6.83 MPa
990 psi
post cured- 4 hours at 204°C
9.404 MPa
1364 psi
post cured- 2 hours at 177°C
10.1 MPa
1460 psi
as molded
Tensile Strength, Yield 2.03 MPa
295 psi
200%, post cured- 4 hours at 204°C
2.28 MPa
330 psi
at 200%, as molded
2.50 MPa
362 psi
at 200%, post cured- 2 hours at 177°C
Elongation at Break 526 %
526 %
post cured- 4 hours at 204°C
596 %
596 %
post cured- 2 hours at 177°C
655 %
655 %
as molded
Tear Strength 30.3 kN/m
173 pli
as molded; Die B
32.4 kN/m
185 pli
post cured- 4 hours at 204°C; Die B
35.9 kN/m
205 pli
post cured- 2 hours at 177°C; Die B