Material Notes:
Multi-Pro 5014 CU W is a calcium carbonate reinforced PP concentrate with balanced impact and stiffness properties. This product is specially formulated for lawn furniture, suitable for outdoor exposure. Data obtained with 1:1 dilution of PPH MFI 14.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955-89
Melt Flow 14 g/10 min
14 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 26.6 MPa
3860 psi
ASTM D638-95
Elongation at Break >= 150 %
>= 150 %
ASTM D638-95
Flexural Strength 41.4 MPa
6000 psi
ASTM D790-95
Flexural Modulus 1.793 GPa
260.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 4.81 J/cm
9.01 ft-lb/in
ASTM D256-93a
Gardner Impact 8.20 J
6.05 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648-95