Material Notes:
This product is well suited for non-glossy appliance type parts. It replaces ABS at favorable cost performance characteristics and can be made UV stable. This product can be color matched in most custom colors.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955-89
Melt Flow 2.3 g/10 min
2.3 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.4 MPa
2810 psi
ASTM D638-95
Elongation at Break 900 %
900 %
ASTM D638-95
Flexural Strength 31.0 MPa
4500 psi
ASTM D790-92
Flexural Modulus 2.379 GPa
345.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256-93a
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420-93