Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Melt Flow 2.05 g/10 min
2.05 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.3 MPa
2800 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Strength 24.5 MPa
3550 psi
ASTM D790
Flexural Modulus 0.979 GPa
142 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
73°F; ASTM D256
Gardner Impact 27.12 J
20.00 ft-lb
ASTM D3029