Multibase Multi-Pro® 0112 Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 0112 Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Pro 0112 is a nucleated and antistated polypropylene homopolymer. It is designed for injection molding applications that require superior mold release properties.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792-91
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638-95
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638-95
Elongation at Break 570 %
570 %
ASTM D638-95
Elongation at Yield 10 %
10 %
ASTM D638-95
Tensile Modulus 1.52 GPa
220 ksi
Secant at 1% strain; ASTM D-638-95
Flexural Modulus 1.241 GPa
180.0 ksi
Secant 1% strain; ASTM D-790-95
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256-93a