Multibase Multi-Flex® TPO DEFA 1037

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO DEFA 1037.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955-89
Melt Flow 2.5 g/10 min
2.5 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 13.1 MPa
1900 psi
ASTM D638-95
Elongation at Break 500 %
500 %
ASTM D638-95
Elongation at Yield 24 %
24 %
ASTM D638-95
Flexural Modulus 0.2759 GPa
40.02 ksi
Secant 1%; ASTM D-790-95
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C
115 °F
ASTM D648-95
Users viewing this material also viewed the following: