Multibase Multi-Flex® TPO D-6509

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D-6509.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex® A-6509 thermoplastic elastomer blend is designed to provide processors with cost effective compounds with excellent tear strength, tensile strength and high elongation. Multi-Flex® A-6509 features good injection molding and extrusion flow characteristics. Parison strength is excellent for blow molding applications. Pre-drying prior to processing is usually not necessary as with other thermoplastic elastomers.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955-89
Melt Flow 9.0 g/10 min
9.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D638-95
Elongation at Break 1700 %
1700 %
ASTM D638-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Tear Strength 47.3 kN/m
270 pli
ASTM D624-95