Material Notes:
Multi-Flex® D 6507 is a mineral filled TPO polypropylene compound designed for applications requiring high impact and moderate stiffness.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792-91
Melt Flow 7.0 g/10 min
7.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 16.8 MPa
2440 psi
ASTM D638-95
Elongation at Break 830 %
830 %
ASTM D638-95
Flexural Modulus 1.448 GPa
210.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.920 J/cm
1.72 ft-lb/in
ASTM D256-93a
Gardner Impact 15.8 J
11.7 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648-95