Material Notes:
This product was developed for soft touch airbag covers and contains Kraton G form Shell. The fogging test value is 70% according to ASTM GM 9305P. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792
Melt Flow 10 - 20 g/10 min
10 - 20 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
10 sec; ASTM D-2240
Tensile Strength, Ultimate 2.80 MPa
406 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength Test 17.5 - 24.5
17.5 - 24.5
ASTM D624