Material Notes:
Flame retardant thermoplastic rubber based on Shell's Kraton G polymers, manufactured under Shell's license. Product exhibits VO rating. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.30 MPa
1200 psi
ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Flexural Strength 2.40 MPa
348 psi
ASTM D790
Flexural Modulus 0.0620 GPa
8.99 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0