Material Notes:
Multi-Flex® D 4310 Natural was designed to replace Himont's CA 53 G material. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0129 cm/cm
0.0129 in/in
ASTM D955
Melt Flow 7.5 g/10 min
7.5 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
10 sec; ASTM D-2240
Tensile Strength, Ultimate 17.2 MPa
2490 psi
ASTM D638
Elongation at Break 1300 %
1300 %
ASTM D638
Flexural Strength 14.0 MPa
2030 psi
ASTM D790
Flexural Modulus 0.445 GPa
64.5 ksi
method 1, Proc.B; ASTM D-790
Gardner Impact 23.2 J
17.1 ft-lb
ASTM D3029
Tear Strength 96.3 kN/m
549 pli
ASTM D624