Multibase Multi-Flex® TPE D 4107

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE D 4107.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is UV stabilized for automotive applications, like fender guards and airbags. The Xenon Arc is 2.5 Delta E, ASTM SAE J1960 1240 KJ/m². Passes Impact resistance test ASTM GM 9032 P at 3.4 J at -30°C. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 6.0 - 12 g/10 min
6.0 - 12 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
10 sec; ASTM D-2240
Tensile Strength, Ultimate 10.3 - 14.5 MPa
1490 - 2100 psi
ASTM D638
Elongation at Break 500 - 700 %
500 - 700 %
ASTM D638
Flexural Strength 6.90 - 8.60 MPa
1000 - 1250 psi
ASTM D790
Tear Strength Test 65 - 88
65 - 88
ASTM D624
Optical Properties Metric English Comments
Gloss 34 - 42 %
34 - 42 %