Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 9002-SR BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 9002-SR BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.90 MPa
1290 psi
ASTM D412
Elongation at Break 527 %
527 %
ASTM D412
Flexural Modulus 0.117 GPa
17.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 3.40 kN/m
19.4 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved