Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 8000 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8000 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.046 g/cc
0.03779 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0132 cm/cm
0.0132 in/in
ASTM D955
Melt Flow 0.60 g/10 min
0.60 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
10 sec; ASTM D-2240
Tensile Strength, Ultimate 11.8 MPa
1710 psi
ASTM D412
Elongation at Break 671 %
671 %
ASTM D412
Tear Strength 51.0 kN/m
291 pli
ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
Users viewing this material also viewed the following: