Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 30 - 50 g/10 min
30 - 50 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 3.00 MPa
>= 435 psi
ASTM D412
Elongation at Break >= 250 %
>= 250 %
ASTM D412
Flexural Modulus 0.0620 GPa
8.99 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 32.5 kN/m
185 pli
ASTM D624