Multibase Multi-Flex® TPE A 7321 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7321 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 39 g/10 min
39 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
10 sec; ASTM D-2240
Tensile Strength, Ultimate 5.40 MPa
783 psi
ASTM D412
Elongation at Break 565 %
565 %
ASTM D412
Flexural Modulus 0.0620 GPa
8.99 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 29.8 kN/m
170 pli
ASTM D624