Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
10 sec; ASTM D-2240
Tensile Strength, Ultimate 7.60 MPa
1100 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 35.0 kN/m
200 pli
ASTM D624
Compression Set 19 %
19 %
for 70 hours at 23°C; ASTM 395
29 %

@Temperature 70.0 °C
29 %

@Temperature 158 °F
for 70 hours at 70°C; ASTM 395
45 %

@Temperature 100 °C
45 %

@Temperature 212 °F
70 hours at 100°C; ASTM 395